1
GATE ME 2016 Set 1
MCQ (Single Correct Answer)
+1
-0.3
The part of a gating system which regulates the rate of pouring of molten metal is
A
pouring basin
B
runner
C
choke
D
ingate
2
GATE ME 2016 Set 3
MCQ (Single Correct Answer)
+1
-0.3
Equal amounts of a liquid metal at the same temperature are poured into three moulds made of steel, copper and aluminum. The shape of the cavity is a cylinder with $$15$$ $$mm$$ diameter. The size of the moulds are such that the outside temper-ature of the moulds do not increase appreciably beyond the atmospheric temperature during solidification. The sequence of solidification in the mould from the fastest to slowest is

(Thermal conductivities of steel, copper and aluminum are $$60.5, 401$$ and $$237$$ $$W/m$$-$$K,$$ respectively. Specific heats of steel, copper and aluminum are $$434, 385$$ and $$903$$ $$J/kg$$-$$K,$$ respectively. Densities of steel, copper and aluminum are $$7854, 8933$$ and $$2700$$ $$kg/{m^3},$$ respectively.)

A
Copper $$-$$ Steel $$-$$ Aluminium
B
Aluminium $$-$$ Steel $$-$$ Copper
C
Copper $$-$$ Aluminium $$-$$ Steel
D
Steel $$-$$ Copper $$-$$ Aluminium
3
GATE ME 2015 Set 3
MCQ (Single Correct Answer)
+1
-0.3
In full mould (cavity-less) casting process, the Pattern is made of
A
Expanded polystyrene
B
Wax
C
Epoxy
D
Plaster of Paris
4
GATE ME 2014 Set 3
MCQ (Single Correct Answer)
+1
-0.3
Match the casting defects (Group A) with the probable causes (Group B): GATE ME 2014 Set 3 Production Engineering - Casting Question 51 English
A
$$P - 1,\,\,Q - 3,\,\,R - 2,\,\,S - 4$$
B
$$P - 4,\,\,Q - 3,\,\,R - 2,\,\,S - 1$$
C
$$P - 3,\,\,Q - 4,\,\,R - 2,\,\,S - 1$$
D
$$P - 1,\,\,Q - 2,\,\,R - 4,\,\,S - 3$$

GATE ME Subjects

Browse all chapters by subject

Turbo Machinery