1
GATE ME 2011
MCQ (Single Correct Answer)
+1
-0.3
The maximum possible draft in cold rolling of sheet increases with the
A
increase in coefficient of friction
B
decrease in coefficient of friction
C
decrease in roll radius
D
increase in roll velocity
2
GATE ME 2003
MCQ (Single Correct Answer)
+1
-0.3
Cold working of steel is defined as working
A
at its re-crystallization temperature
B
above its re-crystallization temperature
C
below its re-crystallization temperature
D
at two thirds of the melting temperature of the metal
3
GATE ME 2002
MCQ (Single Correct Answer)
+1
-0.3
Ductility of material with work hardening
A
Increases
B
Decreases
C
Remains same
D
Unpredictable
4
GATE ME 2002
MCQ (Single Correct Answer)
+1
-0.3
Hot rolling of mild steel is carried out
A
at recrystallisation temp
B
between $$100C$$ to $$150C$$
C
below recrystallisation temp
D
above recrystallisation temp
GATE ME Subjects
Turbo Machinery
EXAM MAP
Joint Entrance Examination
JEE MainJEE AdvancedWB JEEBITSAT
Medical
NEET
Graduate Aptitude Test in Engineering
GATE CSEGATE ECEGATE EEGATE MEGATE CEGATE PIGATE IN