1
GATE ME 1996
Subjective
+2
-0
GATE ME 1996 Production Engineering - Metal Forming Question 26 English
2
GATE ME 1996
MCQ (Single Correct Answer)
+2
-0.6
A wire of $$0.1mm$$ diameter is drawn from a rod of $$15mm$$ diameter dies giving reductions of $$20\% $$, $$40\% $$ and $$80\% $$ are available. For minimum error in the final size, the number of stages and reduction at each stage respectively would be
A
$$3$$ stages and $$80\% $$ reduction for all three stages
B
$$4$$ stages and $$80\% $$ reduction for first three stages followed by a finishing stage of $$20\% $$ reduction
C
$$5$$ stages and reduction of $$80\% $$, $$80\% $$, $$40\% $$, $$40\% $$, $$20\% $$ in sequence
D
None of the above
3
GATE ME 1996
MCQ (More than One Correct Answer)
+1
-0
Preheating before welding is done to
A
Make the steel softer
B
Burn away oil, grease, etc., from the plate surface
C
Prevent cold cracks
D
Prevent plate distortion
4
GATE ME 1996
Subjective
+2
-0
GATE ME 1996 Production Engineering - Welding Process Question 35 English
EXAM MAP
Medical
NEETAIIMS
Graduate Aptitude Test in Engineering
GATE CSEGATE ECEGATE EEGATE MEGATE CEGATE PIGATE IN
Civil Services
UPSC Civil Service
Defence
NDA
Staff Selection Commission
SSC CGL Tier I
CBSE
Class 12