The thickness of the blank needed to produce, by power spinning a missile cone of thickness $$1.5mm$$ and half cone angle $$30deg$$
A
$$3.0mm$$
B
$$2.5mm$$
C
$$2.0mm$$
D
$$1.5mm$$
2
GATE ME 1992
Subjective
+2
-0
Component process GATE ME 1992 Production Engineering - Machining Question 17 English
3
GATE ME 1992
Fill in the Blanks
+1
-0
In horizontal milling process ............................ (up/down) milling provides better surface finish and .............................. Up/down ) milling provide longer tool life.
4
GATE ME 1992
Subjective
+5
-0
In an orthogonal cutting operation on a work piece of width $$2.5mm,$$ the uncut chip thickness was $$0.25$$ $$mm$$ and the tool rake angle was $$0$$(zero) degrees. It was observed that the chip thickness was $$1.25mm.$$ The cutting force was measured to be $$900N$$ and the thrust force was found to be $$450N.$$ Find the mean shear strength of the work piece material and if the coefficient of friction between the chip and the tool was $$0.5,$$ what is the machining constant.
EXAM MAP
Medical
NEETAIIMS
Graduate Aptitude Test in Engineering
GATE CSEGATE ECEGATE EEGATE MEGATE CEGATE PIGATE IN
Civil Services
UPSC Civil Service
Defence
NDA
Staff Selection Commission
SSC CGL Tier I
CBSE
Class 12