Consider the following steps in forging a connecting rod from the bar stock
$$1.$$ blocking $$\,\,\,\,\,\,\,\,\,$$ $$\,\,\,\,\,\,\,\,\,$$ $$\,\,\,\,\,\,\,\,\,$$$$2.$$ trimming
$$3.$$ finishing$$\,\,\,\,\,\,\,\,\,$$ $$\,\,\,\,\,\,\,\,\,$$ $$\,\,\,\,\,\,\,\,\,$$ $$4.$$ edging
Select the correct sequence of these operations using the codes given below
2
GATE PI 2003
MCQ (Single Correct Answer)
+2
-0.6
Cold working produces the following effects
$$1.$$$$\,\,\,\,\,\,\,\,\,\,\,\,\,\,$$ Stress are set up in the material
$$2.$$$$\,\,\,\,\,\,\,\,\,\,\,\,\,\,$$ Grain structure get distorted
$$3.$$$$\,\,\,\,\,\,\,\,\,\,\,\,\,\,$$ Strength and hardness of the metal are decreased
$$4.$$$$\,\,\,\,\,\,\,\,\,\,\,\,\,\,$$ Surface finish is reduced
3
GATE PI 2003
MCQ (Single Correct Answer)
+5
-1.5
In a single pass flat rolling operation, a $$400mm$$ wide steel strip having a thickness of $$10mm$$ is reduced to $$8mm$$ by using a roll of $$600mm$$ diameter.
The roll-strip contact length is
4
GATE PI 2003
MCQ (Single Correct Answer)
+5
-1.5
In a single pass flat rolling operation, a $$400$$ $$mm$$ wide steel strip having a thickness of $$10mm$$ is reduced to $$8$$ $$mm$$ by using a roll of $$600mm$$ diameter.
Considering the situation for a maximum draft of the process, what is the coefficient of friction?
Paper analysis
Total Questions
Casting
4
Joining of Materials
9
Machine Tools and Machining
13
Metal Forming
8
Metrology
1
More papers of GATE PI
GATE PI 2017
GATE PI 2016
GATE PI 2015
GATE PI 2014
GATE PI 2013
GATE PI 2012
GATE PI 2011
GATE PI 2010
GATE PI 2009
GATE PI 2008
GATE PI 2007
GATE PI 2006
GATE PI 2005
GATE PI 2004
GATE PI 2003
GATE PI 2002
GATE PI 2001
GATE PI 1995
GATE PI 1994
GATE PI 1993
GATE PI 1992
GATE PI 1991
GATE PI 1990
GATE PI 1989
GATE PI
Papers
2017
2016
2015
2014
2013
2012
2011
2010
2009
2008
2007
2006
2005
2004
2003
2002
2001
1995
1994
1993
1992
1991
1990
1989