1
GATE PI 2011
MCQ (Single Correct Answer)
+2
-0.6
The number of defective produced by a six sigma process (in Parts per million) is
2
GATE PI 2011
MCQ (Single Correct Answer)
+2
-0.6
During orthogonal machining of a mild steel specimen with a cutting tool of zero rake angle, the following data is obtained:
Uncut chip thickness $$=0.25$$ $$mm$$
Chip thickness $$=0.75$$ $$mm$$
Width of cut $$=2.5$$ $$mm$$
Normal force $$=950$$ $$N$$
Thrust force $$=475$$ $$N$$
Uncut chip thickness $$=0.25$$ $$mm$$
Chip thickness $$=0.75$$ $$mm$$
Width of cut $$=2.5$$ $$mm$$
Normal force $$=950$$ $$N$$
Thrust force $$=475$$ $$N$$
The ultimate shear stress (in $$N/m{m^2}$$) of the work material is
3
GATE PI 2011
MCQ (Single Correct Answer)
+2
-0.6
Match the following materials with their most appropriate application:
4
GATE PI 2008
MCQ (Single Correct Answer)
+2
-0.6
The quick return mechanism used in shaper has rocker arm drive of length $$200mm.$$ If the crank radius is $$50mm$$ and the offset between crank center and rocker arm pivot is $$20mm,$$ length of the stroke (in meters) is
GATE PI Subjects
Browse all chapters by subject
Engineering Mechanics
Theory of Machines
Thermodynamics
Machine Tools and Machining
Metrology
Joining of Materials
Casting
Engineering Mathematics
Industrial Engineering
Fluid Mechanics
Strength of Materials
Machine Design
Metal Forming