1
GATE PI 2003
MCQ (Single Correct Answer)
+2
-0.6
Match List - I (welding defects) with List - II (causes) and select the correct answer using the codes given below the lists
2
GATE PI 2003
MCQ (Single Correct Answer)
+2
-0.6
A $$900$$ $$mm$$ long steel plate is welded by manual metal arc welding process using welding current of $$150$$ $$A,$$ arc voltage of $$20$$ $$V$$ and welding speed of $$300$$ $$mm/min.$$ If the process efficiency of is $$0.8$$ and surface resistance is $$36$$ micro-ohm, the heat input will be
3
GATE PI 2002
MCQ (Single Correct Answer)
+2
-0.6
In spot pulsed laser welding of aluminium plates (density $$ = 2700kg/{m^3},$$ specific heat $$=896J/kg,$$ melting temp $$=933K,$$ latent heat of melting $$ = 398\,\,kJ/kg)$$ at a temp of $${30^ \circ }C,$$ pulse with energy of $$0.5J$$ is focused onto an area of $$0.05m{m^2}.$$ If the entire energy is coupled into the material, what will be the depth of weld assuming the $$CS$$ area of the weld is circular and is uniform throughout its depth and only heat conduction in the direction of penetration
4
GATE PI 1993
MCQ (Single Correct Answer)
+2
-0.6
During gas welding of copper sheets a neutral flame was used consuming $$8$$ liters of acetylene. But the weld was found to be defective. So it was re-welded using an oxidizing flame. The likely consumption of oxygen in liters will be
GATE PI Subjects
Browse all chapters by subject
Engineering Mechanics
Theory of Machines
Thermodynamics
Machine Tools and Machining
Metrology
Joining of Materials
Casting
Engineering Mathematics
Industrial Engineering
Fluid Mechanics
Strength of Materials
Machine Design
Metal Forming