1
GATE PI 2010
MCQ (Single Correct Answer)
+1
-0.3
Cold shut (lap) may occur in products obtained by:
A
Casting
B
Forging
C
Machining
D
Welding
2
GATE PI 2010
MCQ (Single Correct Answer)
+1
-0.3
Hot die steel, used for large solid dies in drop forging, should necessarily have
A
high strength and high copper content
B
High hardness and low hardenability
C
High toughness and low thermal conductivity
D
High hardness and high thermal conductivity
3
GATE PI 2010
MCQ (Single Correct Answer)
+2
-0.6
During open die forging process using two flat and parallel dies, a solid steel disc of initial radius $$({R_{IN}})\,\,200mm$$ and Initial height $$({H_{IN}})\,\,50mm$$ attains a height $$({H_{FN}})$$ of $$30mm$$ and radius of $${R_{FN}}$$. Along the die-disc interfaces

(i) The coefficient of friction $$\left( \mu \right)$$ is :
$$\,\,\,\,\,\,\,\mu = 0.35\left[ {1 + {e^{ - {R_{IN}}/{R_{FN}}}}} \right]$$

(ii) In the region $${R_{SS}}\,\, \le \,\,r\,\, \le \,\,{R_{FN}},$$ sliding friction prevails and
$$\,\,\,\,\,\,P = \sqrt 3 .K.{e^{2\mu \left( {{R_{IN}} - r} \right)/{H_{FN}}}}$$ and $$\tau = \mu \,p$$

Where $$p$$ and $$\tau $$ are the normal and the shear stress respectively; $$K$$ is the shear yield strength of steel and $$r$$ is the radial distance of any point
(i) In the region $$0\, \le \,r\, \le \,{R_{IN}}.$$ sticking condition prevails

The value of $$RSS$$ (in $$mm$$ ), where sticking condition changes to sliding friction is

A
$$241.76$$
B
$$254.55$$
C
$$265.45$$
D
$$278.20$$
4
GATE PI 2010
MCQ (Single Correct Answer)
+2
-0.6
In a rolling process, the roll separating force can be decreased by
A
Reducing the roller diameter
B
Increasing friction between the rolls and the metal
C
Reducing front tension to rolled material
D
Providing back up rollers
EXAM MAP
Medical
NEETAIIMS
Graduate Aptitude Test in Engineering
GATE CSEGATE ECEGATE EEGATE MEGATE CEGATE PIGATE IN
Civil Services
UPSC Civil Service
Defence
NDA
Staff Selection Commission
SSC CGL Tier I
CBSE
Class 12