1
GATE PI 1989
MCQ (Single Correct Answer)
+1
-0.3
Green strength in powder metallurgy refers to the strength of
A
original material in the bulk form
B
the powder before compaction
C
The powder after compaction
D
The powder after sintering and cooling
2
GATE PI 1989
MCQ (Single Correct Answer)
+2
-0.6
Shrinkage allowance on pattern is provided to compensate for shrinkage when
A
The temperature of liquid metal drops from pouring to freezing temperature
B
The metal changes from liquid to solid state at freezing temperature
C
The temperature of solid phase drops from freezing to room temperature
D
The temperature of metal drops from pouring to room temperature
3
GATE PI 1989
Subjective
+2
-0
What is the velocity of the steel at the bottom of the sprue if the sprue height is $$30$$ $$cm$$? Assume the frictional and other losses to be $$20\% $$
4
GATE PI 1989
MCQ (Single Correct Answer)
+5
-1.5
Molten aluminium was poured in a sand mold and the thickness of solid skin formed after $$20$$ seconds and $$50$$ seconds were fond to be $$3mm$$ and $$4.5mm$$ respectively. What would be the thickness of the solid skin at the end of $$100$$ seconds after pouring?
A
$$5.5mm$$
B
$$6.19mm$$
C
$$7.1mm$$
D
none
EXAM MAP
Medical
NEETAIIMS
Graduate Aptitude Test in Engineering
GATE CSEGATE ECEGATE EEGATE MEGATE CEGATE PIGATE IN
Civil Services
UPSC Civil Service
Defence
NDA
Staff Selection Commission
SSC CGL Tier I
CBSE
Class 12