1
GATE PI 2010
MCQ (Single Correct Answer)
+1
-0.3
Solidification time of a metallic alloy casting is
A
Directly proportional to its surface area
B
Inversely proportional to the specific heat of the cast material
C
Inversely proportional to the thermal diffusivity of the mould material
D
Inversely proportional to the pouring temp
2
GATE PI 2009
MCQ (Single Correct Answer)
+1
-0.3
Hot chamber die casting is NOT suited for
A
Lead and its alloys
B
zinc and its alloys
C
Tin and its alloys
D
Aluminium and its alloys
3
GATE PI 2008
MCQ (Single Correct Answer)
+1
-0.3
In hollow cylindrical parts made by centrifugal casting, the density of the part is
A
Maximum at the outer region
B
Maximum at the inner region
C
Maximum at the mid point between outer and inner surfaces
D
Uniform throughout
4
GATE PI 2006
MCQ (Single Correct Answer)
+1
-0.3
Cold shut is a defect in casting due to
A
sand sliding from the cope surface
B
internal voids or surface depression due to excessive gas trapped
C
discontinuity resulting from hindered contraction
D
two streams of material that are too cold to fuse properly
EXAM MAP
Medical
NEETAIIMS
Graduate Aptitude Test in Engineering
GATE CSEGATE ECEGATE EEGATE MEGATE CEGATE PIGATE IN
Civil Services
UPSC Civil Service
Defence
NDA
Staff Selection Commission
SSC CGL Tier I
CBSE
Class 12